What is LR EH46 steel plate?

Dec 26, 2025 ترك رسالة

LR EH46 steel plate is a high-strength, low-temperature grade shipbuilding steel certified by Lloyd's Register (LR), known for excellent toughness, strength (Yield ~420 MPa, Tensile ~530-680 MPa), and good weldability, primarily used for hulls, offshore structures, and large vessels operating in harsh, cold marine environments. The 'E' signifies its suitability for low temperatures, 'H' denotes high strength, and '46' indicates its minimum yield strength in kg/mm², making it ideal for critical structural components needing impact resistance.

 

 

LR EH46 extra high Strength Chemical Composition

C

P

S

N

LR EH46

0.20

0.55

1.70

0.030

0.030

0.015

0.020

V

0.02-0.05

0.03-0.10

0.02

 

 

 

 

 

 

LR EH46 extra high strength property

 

Energy 1

Energy 2

LR EH46

-40

J

J

t<=50

460

570-720

19%

31

46

50<t<=70

460

570-720

19%

31

46

70<t<=100

460

570-720

19%

31

46

Note: Energy 1 is transverse impact test, Energy 2 is longitudinal

 

 

Equivalent steel grade of LR/EH46

NV E460

GL-E460

AB/EQ47

BV/E460

CCS/E460

K E47

R E47

RI/E460

 

Standard: LR (Lloyd's Register) Shipbuilding Steel Standard.

Strength: Higher strength grade, offering superior performance over basic grades like LR Grade A or D.

Toughness: Excellent impact toughness, even at low temperatures (e.g., -40℃), crucial for marine safety.

Applications: Ship hulls, offshore platforms, drilling rigs, pipe joints, and other demanding marine engineering projects.

Composition & Properties: Carefully controlled chemistry (e.g., low Carbon, specific Silicon/Manganese) and heat treatment ensure its mechanical properties, with minimum elongation often around 18%.