A302 Grade B steel plates standard specification for pressure vessel plates in alloy steel, manganese molybdenum and manganese-molybdenum-nickel.
A302 Grade B steel plate shall be normally supplied in the as-rolled condition. Plates may be ordered normalized or stress relieved, or both. If A 302 Grade B above 50mm in thickness shall be normalized.
Supplementary Technology: HIC Test|NACE MR0175|Z15|Z25|Z35 |
Thickness: 6MM to 300MM,
Width: 1500mm to 4050mm,
Length: 3000mm to 15000mm
|
A302 Grade B Chemical Composition |
|||||||
|
% |
% |
% |
% |
||||
|
25mm or under |
0.2 |
1.15-1.50 |
0.15-0.40 |
0.035 |
|||
|
25-50mm |
0.23 |
1.07-1.62 |
0.13-0.45 |
||||
|
over 50mm |
0.25 |
|
|
|
|
||
|
|
|
% |
% |
% |
|||
|
|
|
0.45-0.60 |
… |
0.035 |
|||
|
|
|
0.41-0.64 |
… |
||||
Carbon Equivalent: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%
A302 Grade B Mechanical Property
|
Mechanical Property of A302 Grade B steel plate |
A302 Grade B |
|
80-100 [550-690] |
|
|
50 [345] |
|
|
Elongation in 8 in. [200 mm], min, % |
15 |
|
Elongation in 2 in. [50 mm], min, % |
18 |
|
Equivalent steel grade of A302 Grade B |
|||||||
|
|
|
|
|
|
Gr.27,31 |
|
|